In this paper, AlON phosphors doped with Ce3+ are prepared by solid-state reaction method. Phases, microstructures and optical properties of the synthesized phosphors are characterized by X-ray diffraction and scanning electron microscopy and photoluminescence. The results indicate that AlON3+:Ce phosphors emit the blue light centered at 390 nm under the excitation of 305 nm. The emission intensity of AlON:Ce3+ at 150 ℃ is about 86% of that measured at room temperature. It demonstrates that the AlON:Ce3+ has a great potential in applications of high-density white light-emitting diodes.
-
Keywords:
- photoluminescence /
- concentration quenching /
- thermal stability
[1] Yamamoto H 2010 Proc. SPIE 7598 759808
[2] He X H, Lian N, Sun J H, Guan M Y 2009 J. Mater. Sci. 44 4763
[3] Xie R J, Hirosaki N, Mitomo M, Uheda K, Suehiro T, Xu X, Yamamoto Y, Sekiguchi T 2005 J. Phys. Chem. B 109 9490
[4] Xie R J, Hirosaki N, Mitomo M, Suehiro T, Xu X, Tanaka H 2005 J. Am. Ceram. Soc. 88 2883
[5] Kikkawa S, Nagasaka K, Takeda T, Bailey M, Sakurai T, Miyamoto Y 2007 J. Solid State Chem. 180 1984
[6] Taguchi T 2008 IEEJ Trans. 3 21
[7] Xie R J, Hirosaki N, Liu X J, Takeda T, Li H L 2008 Appl. Phys. Lett. 92 201905
[8] Yin L J, Xu L Y, Hao Y, Xie Y F, Wang L X, Yang X F 2009 Matter Lett. 6 1511
[9] Yin L J, Yu W, Xu X, Hao L Y 2012 J. Lumin. 132 671
[10] Zhang F, Chen S, Chen J F, Zhang H L, Li J, Liu J, Wang S W 2012 J. Appl. Phys. 111 083532
[11] Hartnett T M, Maguire E A, Gentilman R L, Corbin N D, Mc-Cauley J W 1982 Cera. Eng. Sci. Proc. 3 67
[12] Pan L, Lu T C, Su R, Wang Y Z, Qi J Q, Fu J, Zhang Y, He D W 2010 Acta Phys. Sin. 59 2027 (in Chinese) [潘磊, 卢铁城, 苏锐, 王跃忠, 齐建起, 付佳, 张燚, 贺端维 2010 59 2027]
[13] Li P L, Xu Z, Zhao S L, Wang Y S, Zhang F J 2012 Chin. Phys. B 21 047803
-
[1] Yamamoto H 2010 Proc. SPIE 7598 759808
[2] He X H, Lian N, Sun J H, Guan M Y 2009 J. Mater. Sci. 44 4763
[3] Xie R J, Hirosaki N, Mitomo M, Uheda K, Suehiro T, Xu X, Yamamoto Y, Sekiguchi T 2005 J. Phys. Chem. B 109 9490
[4] Xie R J, Hirosaki N, Mitomo M, Suehiro T, Xu X, Tanaka H 2005 J. Am. Ceram. Soc. 88 2883
[5] Kikkawa S, Nagasaka K, Takeda T, Bailey M, Sakurai T, Miyamoto Y 2007 J. Solid State Chem. 180 1984
[6] Taguchi T 2008 IEEJ Trans. 3 21
[7] Xie R J, Hirosaki N, Liu X J, Takeda T, Li H L 2008 Appl. Phys. Lett. 92 201905
[8] Yin L J, Xu L Y, Hao Y, Xie Y F, Wang L X, Yang X F 2009 Matter Lett. 6 1511
[9] Yin L J, Yu W, Xu X, Hao L Y 2012 J. Lumin. 132 671
[10] Zhang F, Chen S, Chen J F, Zhang H L, Li J, Liu J, Wang S W 2012 J. Appl. Phys. 111 083532
[11] Hartnett T M, Maguire E A, Gentilman R L, Corbin N D, Mc-Cauley J W 1982 Cera. Eng. Sci. Proc. 3 67
[12] Pan L, Lu T C, Su R, Wang Y Z, Qi J Q, Fu J, Zhang Y, He D W 2010 Acta Phys. Sin. 59 2027 (in Chinese) [潘磊, 卢铁城, 苏锐, 王跃忠, 齐建起, 付佳, 张燚, 贺端维 2010 59 2027]
[13] Li P L, Xu Z, Zhao S L, Wang Y S, Zhang F J 2012 Chin. Phys. B 21 047803
Catalog
Metrics
- Abstract views: 6092
- PDF Downloads: 673
- Cited By: 0