  • 通过熔体快淬方法获得Pr(Fe1-xCox)2合金条带,经过X射线衍射、差示扫描量热计和磁性测量对其结构、磁性和热稳定性进行了研究.发现当Co的含量x大于0.2时才可能获得Pr(Fe,Co)2立方Laves相化合物.对Pr(Fe0.6Co0.4)2合金,在快淬速度为30m/s时,条带由Pr2(Fe,Co)17,Pr(Fe,Co)2和富稀土相组成;在速度为40m/s时,获得了几乎单相的Pr(Fe0.6Co0.4)2化合物,其居里温度为305℃;在速度为45m/s时,除了Pr(Fe0.6Co0.4)2化合物外,还存在少量的非晶相.Pr(Fe0.6Co0.4)2化合物在770℃以上发生分解.用40m/s快淬纳米晶粉胶粘磁体有大的磁致伸缩系数(λ∥-λ⊥=140×10-6)和高的硬磁性能(iHc=398kA/m).

     

    Pr(Fe1-xCox)2 ribbons have been prepared by melt-spinning method. Their structure, magnetic properties and thermal stability are investigated. It is found that Pr(Fe,Co)2 cubic Laves phase can form only when x≥0.2 at wheel speed of 45m/s. For Pr(Fe0.6Co0.4)2 alloy, at wheel speed of 30m/s, the ribbon consistes of a mixture of Pr2(Fe,Co)17, Pr(Fe,Co)2 and rare earth-rich phase. Almost Pr(Fe0.6Co0.4)2 compound a small amount of amorphous phase is observed at wheel speed up to 45m/s. Pr(Fe0.6Co0.4)2 compound becomes unstable above 770℃. The resub-bonded Pr(Fe0.6Co0.4)2 nanocrystalline compound which is obtained at wheel speed of 40m/s combines high magnetostriction (λ∥-λ⊥=140×10-6), with significant magnetic coercivity, iHc=398kA/m.

     

    目录

    /

    返回文章
    返回
    Baidu
    map